Title: | Compressive Strength of Re-Vibrated Concrete Containing Locust Bean Epicarp Extract and Bida Natural Stone As Coarse Aggregate |
Authors: | Shehu, M. Abbas, B. A Abubakar, M. A. |
Keywords: | Bida natural stone Locust Bean Epicarp Extract Ordinary Portland Cement British standard |
Issue Date: | 2021 |
Publisher: | Proceedings of 6th National Engineering Conference Organized by the Nigerian Institute of mechanical engineer, Minna chapter |
Series/Report no.: | Proceedings of 6th National Engineering Conference Organized by the Nigerian Institute of mechanical engineer, Minna chapter; |
Abstract: | Abstract: The compressive strength of re-vibrated concrete containing locust bean epicarp extract and Bida Natural Stone (BNS) as coarse aggregate. one hundred and sixty-eight concrete cubes were produced in six batches, in which twenty- eight cubes was produce in each of this batches. However, two of these batches were at 0% LBEE + 100% OPC and 100% LBEE + 100%OPC, the rest are at cement reduction content of 5, 10, 15 and 20%, but all the others concrete mix ingredients remained constant. The epicarp used was at constant concentration of 0.1kg/l. The concrete mix adopted was 1 :2 :4 using ordinary Portland cement with water cement ratio of 0.5. The preliminary results show that the aggregate falls within the BS requirement. Concrete cubes were cast with re-vibration time lag intervals of 10minute for the period of 60minute re-vibration process and cured for 7 and 28days. When tested for their respective compressive strength, the result obtained shows that there is increase in compressive strength with increase in re- vibration time lag. The result also shows that introduction of LBEE increase compressive strength of concrete produced despite cement reduction up to 20%. The maximum compressive strength for all batches at 28days cu ring was obtained at 60 minutes. For batch B at 40-minute re-vibration time interval for and water cement ratio of 0.5 at constant concentration LBEE of 0.1kg/l. The maximum attained compressive strength for 28days curing was 36.27N/mm2 for B (100% LBEE + 100% OPC) appears to be higher than 35.42N/mm2 for A (0% LBEE+ 100% OPC). This indicates that the uses of LBEE has adversely enhanced the compressive strength of concrete when re-vibrated. |
URI: | http://repository.futminna.edu.ng:8080/jspui/handle/123456789/28735 |
Appears in Collections: | Civil Engineering |
Files in This Item:
File | Description | Size | Format | |
---|---|---|---|---|
25 NEMECHI SHEHU MUSA.pdf | 1.01 MB | Adobe PDF | View/Open |
Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.